Publication

Structural and nanomechanical properties of a zeolite membrane measured using nanoindentation

Charitidis; CA; Koumoulos; EP; Nikolakis; V; Dragatogiannis; DA


Journal: THIN SOLID FILMS Year: 2012 Volume: 526 Issue: Pages: 168-175